        Injection Molding Unit ABC1000 ABC2000 ABC3000 ABC4000 ABC4100 ABC4200 ABC4300
        drying temperature                     100-120 100-120 100-120 100-120 100-120 100-120 100-120
        drying time                     hrs 4--6 4--6 4--6 4--6 4--6 4--6 4--6
        maximum humidity ratio                     % 0.02 0.02 0.02 0.02 0.02 0.02 0.02
        molding temperature                      ℃  230-270 230-270 230-270 230-270 230-270 230-270 230-270
        mold temperature                     55-80 55-80 55-80 55-80 55-80 55-80  55-80
        back pressure                     MPa 0.3-0.7 0.3-0.7 0.3-0.7 0.3-0.7 0.3-0.7 0.3-0.7 0.3-0.7
        screw rev                     rpm 40-80 40-80 40-80 40-80 40-80 40-80 40-80
        one shot molding ejection volume                     % 50-160 50-160 50-160 50-160 50-160 50-160 50-160
        injection molding pressure                     MPa 50-160 50-160 50-160 50-160 50-160 50-160 50-160


        Injection Molding Recommendations of PC/PET Alloy

        Injection Molding Unit AEC1000 AEC2000 AEC3000 AEC4000
        drying temperature                 100-120 100-120 100-120 100-120
        drying time                 hrs 4--6 4--6 4--6 4--6
        maximum humidity ratio                 % 0.02 0.02 0.02 0.02
        molding temperature                  ℃  240-270 240-270 240-270 240-270
        mold temperature                 60-90 60-90 60-90 60-90
        back pressure                 MPa 0.3-0.7 0.3-0.7 0.3-0.7 0.3-0.7
        screw rev                 rpm 40-80 40-80 40-80 40-80
        one shot molding ejection volume                 % 40-80 40-80 40-80 40-80